Chosun Refractories SAL90CR Special High Alumina brick

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer Chosun Refractories
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chosun Refractories SAL90CR Special High Alumina brick.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Physical Properties Metric English Comments
Bulk Density 3.10 g/cc
0.112 lb/in³
Porosity 16 %
16 %
Mechanical Properties Metric English Comments
Compressive Strength 88.3 MPa
12800 psi
Cold Crushing Strength
Thermal Properties Metric English Comments
CTE, linear 7.10 µm/m-°C

@Temperature 1000 °C
3.94 µin/in-°F

@Temperature 1830 °F
Shrinkage 0.00 %

@Temperature 1500 °C,
Time 7200 sec
0.00 %

@Temperature 2730 °F,
Time 2.00 hour
Component Elements Properties Metric English Comments
Al2O3 90 %
90 %
Cr2O3 4.0 %
4.0 %
Fe2O3 0.30 %
0.30 %
Descriptive Properties Value Comments
Main Application Electric kiln, Cupolar, Incinerator, Various High-temp. furnace
Refractories Under Load(2kg/?,T2?) 1,700 T2
Refractoriness (SK) 41
Copyright © lookpolymers.com All Rights Reserved