Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Physical Properties Metric English Comments
Bulk Density 2.90 g/cc
0.105 lb/in³
Porosity 20 %
20 %
Mechanical Properties Metric English Comments
Compressive Strength 88.3 MPa
12800 psi
Cold Crushing Strength
Thermal Properties Metric English Comments
CTE, linear 7.00 µm/m-°C

@Temperature 1000 °C
3.89 µin/in-°F

@Temperature 1830 °F
Shrinkage 0.00 %

@Temperature 1600 °C,
Time 7200 sec
0.00 %

@Temperature 2910 °F,
Time 2.00 hour
Component Elements Properties Metric English Comments
Al2O3 87 %
87 %
Fe2O3 0.70 %
0.70 %
Descriptive Properties Value Comments
Main Application AI melting kiln, Various Non-ferrous metal melting furnace
Refractories Under Load(2kg/?,T2?) 1,700
Refractoriness (SK) 40