Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Mechanical Properties Metric English Comments
Compressive Strength 17.7 MPa

@Temperature 110 °C,
Time 86400 sec
2560 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
35.3 MPa

@Temperature 1000 °C,
Time 10800 sec
5120 psi

@Temperature 1830 °F,
Time 3.00 hour
Cold Crushing Strength
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 1650 °C
3000 °F
limited
Shrinkage -0.0600 %

@Temperature 110 °C,
Time 86400 sec
-0.0600 %

@Temperature 230 °F,
Time 24.0 hour
0.20 %

@Temperature 1500 °C,
Time 10800 sec
0.20 %

@Temperature 2730 °F,
Time 3.00 hour
Component Elements Properties Metric English Comments
Al2O3 59 %
59 %
SiO2 32 %
32 %