Chosun Refractories PCB-LTT Casting Block

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer Chosun Refractories
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chosun Refractories PCB-LTT Casting Block.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Physical Properties Metric English Comments
Bulk Density 2.30 g/cc
0.0831 lb/in³
Porosity 27 %
27 %
Mechanical Properties Metric English Comments
Compressive Strength 29.4 MPa
4270 psi
Cold Crushing Strength
Component Elements Properties Metric English Comments
Al2O3 60 %
60 %
SiO2 32 %
32 %
Descriptive Properties Value Comments
Characteristics & Main Applications Spalling Resistance Lip Tile