Chosun Refractories L8S Magnesia Carbon Bricks for Ladle Slag Line

Category Ceramic , Oxide , Magnesium Oxide
Manufacturer Chosun Refractories
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chosun Refractories L8S Magnesia Carbon Bricks for Ladle Slag Line.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Physical Properties Metric English Comments
Bulk Density 3.05 g/cc
0.110 lb/in³
Porosity 4.0 %
4.0 %
Mechanical Properties Metric English Comments
Compressive Strength 50.0 MPa
7250 psi
Cold Crushing Strength
Component Elements Properties Metric English Comments
Carbon, C 8.0 %
8.0 %
MgO 82 %
82 %
Descriptive Properties Value Comments
Applications General Use