Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Physical Properties Metric English Comments
Grain Size 75 µm
75 µm
60% <= 0.075 mm
500 µm
500 µm
2% >= 0.50 mm
Mechanical Properties Metric English Comments
Adhesive Bond Strength <= 0.4905 MPa

@Temperature 110 °C,
Time 86400 sec
<= 71.14 psi

@Temperature 230 °F,
Time 24.0 hour
<= 2.943 MPa

@Temperature 400 °C,
Time 10800 sec
<= 426.8 psi

@Temperature 752 °F,
Time 3.00 hour
Component Elements Properties Metric English Comments
Al2O3 <= 60 %
<= 60 %
Carbon, C <= 7.0 %
<= 7.0 %
Descriptive Properties Value Comments
Main Applications Nozzle Setting
Material Al2O3-C
Users viewing this material also viewed the following: