Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Physical Properties Metric English Comments
Bulk Density 3.10 g/cc
0.112 lb/in³
Porosity 10 %
10 %
Mechanical Properties Metric English Comments
Compressive Strength 73.5 MPa
10700 psi
Cold Crushing Strength
Thermal Properties Metric English Comments
CTE, linear 7.00 µm/m-°C

@Temperature 1000 °C
3.89 µin/in-°F

@Temperature 1830 °F
Component Elements Properties Metric English Comments
Al2O3 75 %
75 %
MgO 9.0 %
9.0 %
Descriptive Properties Value Comments
Chemical Analysis(%),SiC+C 7
Refractories Under Load(2kg/?,T2?) 1,700