Chosun Refractories CJS-1 Joint Sheet

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer Chosun Refractories
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chosun Refractories CJS-1 Joint Sheet.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Physical Properties Metric English Comments
Permeability 0.0014

@Temperature 1000 °C,
Time 7200 sec
0.0014

@Temperature 1830 °F,
Time 2.00 hour
Component Elements Properties Metric English Comments
Al2O3 <= 50 %
<= 50 %
Carbon, C <= 3.0 %
<= 3.0 %
Descriptive Properties Value Comments
Compressibility ormal temperature(%) at 1kg/? 20
Compressibility ormal temperature(%) at 2kg/? 40
Compressibility ormal temperature(%) at 3kg/? 50
Main Application Between the bottom of the tundish sliding nozzle and submerged entry nozzle, etc.