Chosun Refractories CER-80 Special Casting Block

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer Chosun Refractories
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chosun Refractories CER-80 Special Casting Block.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Physical Properties Metric English Comments
Bulk Density 2.80 g/cc
0.101 lb/in³
Porosity 13 %
13 %
Mechanical Properties Metric English Comments
Compressive Strength 63.7 MPa
9250 psi
Cold Crushing Strength
Component Elements Properties Metric English Comments
Al2O3 80 %
80 %
SiO2 15 %
15 %
Descriptive Properties Value Comments
Characteristics Resistance to Corrosion, Abrasion, Spalling
Main Applications High temperature Work