Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Physical Properties Metric English Comments
Bulk Density 0.160 g/cc
0.00578 lb/in³
Thermal Properties Metric English Comments
Melting Point 1760 °C
3200 °F
Maximum Service Temperature, Air 1500 °C
2730 °F
Component Elements Properties Metric English Comments
Al2O3 40 %
40 %
Cr2O3 1.8 %
1.8 %
SiO2 58.1 %
58.1 %
Descriptive Properties Value Comments
Typical applications heat seals, packing, appliance and heating apparatus insulation, filter material, asbestos paper substitute