China Tungsten ZP10 Tungsten Carbide

Category Ceramic , Carbide
Manufacturer China Tungsten
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF China Tungsten ZP10 Tungsten Carbide.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Semi-finishing and finishing of steel, steel castings and alloy steel.Information provided by China Tungsten
Physical Properties Metric English Comments
Density 11.95 g/cc
0.4317 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell A 92
92
Flexural Strength 1650 MPa
239000 psi