Material Notes:
It's belong to the fine grain grade. excellent wear resistance. Finishing of cast iron. non-ferrous metals, non-metailic materials and hardened steel. Also suitable for turning and milling.Information provided by China Tungsten
Physical Properties Metric English Comments
Density 14.9 g/cc
0.538 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell A 91.4
91.4
Flexural Strength 1700 MPa
247000 psi