Material Notes:
Coated substrate with higher toughness and slightly less wear resistance than ZC1, for semi-finishing and roughing after coating.Information provided by China Tungsten
Physical Properties Metric English Comments
Density 13.3 - 13.7 g/cc
0.480 - 0.495 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell A 90.5
90.5
Flexural Strength 1800 MPa
261000 psi