Information provided by China Tungsten
Component Elements Properties Metric English Comments
Antimony, Sb <= 0.060 %
<= 0.060 %
Carbon, C <= 0.15 %
<= 0.15 %
Copper, Cu <= 0.80 %
<= 0.80 %
Molybdenum, Mo >= 48 %
>= 48 %
Sulfur, S 0.25 - 0.30 %
0.25 - 0.30 %
Tin, Sn <= 0.070 %
<= 0.070 %
Yttrium, Y <= 50.37 %
<= 50.37 %