China Tungsten YW1 Tungsten Carbide for Cutting Tools

Category Ceramic , Carbide
Manufacturer China Tungsten
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF China Tungsten YW1 Tungsten Carbide for Cutting Tools.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High red hardness, resistant to impact load. A goo grade for general purposes Machining of ordinary steel, cast irons and hard to machining materials such as refractory steel manageress steel, and stainless steelInformation provided by China Tungsten
Physical Properties Metric English Comments
Density 13.0 g/cc
0.470 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell A 92.5
92.5
Flexural Strength 1710 MPa
248000 psi