Material Notes:
High wear resistance and high resistance to plastic deformation Continuous or intermittent cutting of manganese steel and stainless steel.Information provided by China Tungsten
Physical Properties Metric English Comments
Density 13.1 g/cc
0.473 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell A 92
92
Flexural Strength 1800 MPa
261000 psi