China Tungsten YG6A Tungsten Carbide for Cutting Tools

Category Ceramic , Carbide
Manufacturer China Tungsten
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF China Tungsten YG6A Tungsten Carbide for Cutting Tools.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Fine-grained alloy, good; wear resistance. Semi-finishing of chilled cast iron, non-ferrous metals/alloys; semi-finishing and finishing of hardened steel, alloy steel.Information provided by China Tungsten
Physical Properties Metric English Comments
Density 14.9 g/cc
0.538 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell A 92
92
Flexural Strength 1850 MPa
268000 psi