Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

China Tungsten YG610 Tungsten Carbide

Category Ceramic , Carbide
Manufacturer China Tungsten
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF China Tungsten YG610 Tungsten Carbide.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Good thermal strength and high wear resistance .Continuous or intermittent  cutting of cast irons, refractory alloys and quenched steelInformation provided by China Tungsten
Physical Properties Metric English Comments
Density 14.6 g/cc
0.527 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell A 93
93
Flexural Strength 1720 MPa
249000 psi
Users viewing this material also viewed the following: