China Tungsten YG22C Tungsten Carbide

Category Ceramic , Carbide
Manufacturer China Tungsten
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF China Tungsten YG22C Tungsten Carbide.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by China Tungsten
Physical Properties Metric English Comments
Density 13.40 g/cc
0.4841 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell A 84
84
Tensile Strength, Ultimate 2700 MPa
392000 psi
Component Elements Properties Metric English Comments
Cobalt, Co 22 %
22 %
WC 78 %
78 %