China Tungsten ST1460 PM Antifriction Parts

Category Metal , Ferrous Metal
Manufacturer China Tungsten
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF China Tungsten ST1460 PM Antifriction Parts.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by China Tungsten
Physical Properties Metric English Comments
Density 5.80 - 6.30 g/cc
0.210 - 0.228 lb/in³
Component Elements Properties Metric English Comments
Carbon, C 0.50 - 2.0 %
0.50 - 2.0 %
total
Copper, Cu 18 - 22 %
18 - 22 %
Iron, Fe 55 - 60.5 %
55 - 60.5 %
Other <= 3.0 %
<= 3.0 %
Descriptive Properties Value Comments
Oil %, Min 18
Skin Hardness (HR) 50-100