China Tungsten Kmo45-A Molybdenum Concentrate

Category Metal , Nonferrous Metal , Molybdenum Alloy
Manufacturer China Tungsten
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF China Tungsten Kmo45-A Molybdenum Concentrate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by China Tungsten
Component Elements Properties Metric English Comments
Arsenic, As <= 0.050 %
<= 0.050 %
CaO <= 3.0 %
<= 3.0 %
Copper, Cu <= 0.20 %
<= 0.20 %
Lead, Pb <= 0.30 %
<= 0.30 %
Molybdenum, Mo >= 45 %
>= 45 %
Phosphorous, P <= 0.050 %
<= 0.050 %
Potassium, K <= 38.35 %
<= 38.35 %
SiO2 <= 13 %
<= 13 %
Tin, Sn <= 0.050 %
<= 0.050 %