Material Notes:
Copper-Zinc-Lead Alloy (Leaded Brass)Finished product available as bar, rod, forged, or shapes.Chicago Extruded Metal temper codes: H01, H02, M30Information provided by Chicago Extruded Metals
Physical Properties Metric English Comments
Density 8.44 g/cc
0.305 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength 359 MPa
52000 psi
Tensile Strength, Yield 138 MPa
20000 psi
Elongation at Break 45 %
45 %
Machinability 80 %
80 %
UNS C36000 (free-cutting brass) = 100%
Thermal Properties Metric English Comments
Thermal Conductivity 119 W/m-K
828 BTU-in/hr-ft²-°F
Component Elements Properties Metric English Comments
Copper, Cu 58 - 61 %
58 - 61 %
Iron, Fe 0.30 %
0.30 %
Lead, Pb 1.5 - 2.5 %
1.5 - 2.5 %
Other, total 0.50 %
0.50 %
Zinc, Zn 35.7 - 39.7 %
35.7 - 39.7 %
as balance
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000639 ohm-cm
0.00000639 ohm-cm
Copyright © lookpolymers.com All Rights Reserved