Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chicago Extruded Metals BioBrass® UNS C64700 Copper-Silicon Alloy

Category Metal , Nonferrous Metal , Copper Alloy
Manufacturer Chicago Extruded Metals (CXM)
Trade Name BioBrass®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chicago Extruded Metals BioBrass® UNS C64700 Copper-Silicon Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Finished product available as bar, wire, or rod.Chicago Extruded Metal temper codes: H02, M30This alloy is registered with the U.S. EPA as Antimicrobial.Information provided by Chicago Extruded Metals
Physical Properties Metric English Comments
Density 8.91 g/cc
0.322 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength 552 - 621 MPa
80000 - 90000 psi
Tensile Strength, Yield 483 - 517 MPa
70000 - 75000 psi
Elongation at Break 8.0 %
8.0 %
Component Elements Properties Metric English Comments
Copper, Cu 95.81 - 96.81 %
95.81 - 96.81 %
as balance
Iron, Fe 0.10 %
0.10 %
Lead, Pb 0.090 %
0.090 %
Nickel, Ni 1.6 - 2.2 %
1.6 - 2.2 %
Other, total 0.50 %
0.50 %
Silicon, Si 0.40 - 0.80 %
0.40 - 0.80 %
Zinc, Zn 0.50 %
0.50 %
Copyright © lookpolymers.com All Rights Reserved