Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ChevronTexaco Texmar ZF 17 SAE 40

Category Fluid , Lubricant
Manufacturer ChevronTexaco Corp
Trade Name Texmar
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ChevronTexaco Texmar ZF 17 SAE 40.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Texaco Texmar 17 deliver value through:Ability to maximize oil and filter lifeImproved wear controlExtended drainsExtends oil drains in new low oil consumption GE locomotives, reducing oil costsBetter oxidation and viscosity controlBetter alkalinity retentionTexaco Texmar ZF 17 is an outstanding high dispersancy, high alkalinity, 17 base number engine oils for use in diesel engines used in railroad, power generation, oil well drilling, and marine and industrial service requiring a zinc-free oil and Generation 4 LL or Generation 5 lubricant characteristics.Texaco Texmar ZF 17 is manufactured using the highest quality base oils and a nonchlorinated additive package that offers low engine wear and minimizes used oil disposal issues.New engine designs, aimed at reducing operating expenses, operate at higher combustion pressures and higher temperatures which require improved oxidation and viscosity control. In addition, new piston and ring designs call for increased alkalinity reserve to control corrosive wear and deposit formation.Texaco Texmar ZF 17 successfully handles these new requirements by providing outstanding resistance to viscosity increase due to outstanding oxidation and thermal stability, and by providing a high alkalinity level (17 base number, ASTM D 2896).Texaco Texmar ZF 17 is recommended:For use in all railroad-type diesel engines for locomotive, marine equipment, stationary electric generating plants, offshore drilling equipment, and many other applications.Where large medium-speed EMD or GE diesel engines are used for primary power.Texaco Texmar ZF 17 is miscible with competitive railroad type oils and additive systems consistent with engine manufacturers recommended practices.Texaco Texmar ZF 17 provides excellent performance in older locomotive types such as Sulzer, Baldwin, and ALCO.Texaco Engine Oils Texmar 17 is recommended:For use in Caterpillar and other diesel engines operating where sulfated ash levels above 1% are acceptable.Where DDC engines are used for auxiliary power. Detroit Diesel Corporation approves the use of Generation 4 and 5 zinc-free railroad engine oils in these applications.Texaco Texmar ZF 17 meets the performance requirements of:API Service Categories CD1 , CD-II1, CF, CF-2Caterpillar TO-2 (SAE 40)Texaco Texmar ZF 17Is qualified by Electro Motive Division, General Motors, for use in engines operating under EMD factory warrantyIs fully approved by General Electric as Extra Performance LubricantsTypical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing. CPS Number: 222680; MSDS Number: 8615
Physical Properties Metric English Comments
API Gravity 27.9 °
27.9 °
Viscosity Measurement 101
101
Viscosity Index
Kinematic Viscosity at 40°C (104°F) 144 cSt
144 cSt
Kinematic Viscosity at 100°C (212°F) 14.8 cSt
14.8 cSt
Ash 2.0 %
2.0 %
Sulfated Ash, mass %
Thermal Properties Metric English Comments
Pour Point -18.0 °C
-0.400 °F
Flash Point 263 °C
505 °F
Chemical Properties Metric English Comments
Total Base Number 17
17
ASTM D2896
Users viewing this material also viewed the following: