Material Notes:
FeaturesChevron Supreme 100% Synthetic Motor Oils are designed for those drivers who demand the ultimate in engine protection. They provide an extra measure of protection for the investment in a sport utility vehicle (SUV), high performance, or luxury car. Chevron Supreme 100% Synthetic Motor Oils give improved protection to high output, supercharged and turbocharged performance vehicles.Chevron Supreme 100% Synthetic Motor Oils are formulated using 100% synthetic base stocks for the best performance. The improved volatility and stability of synthetic base stocks give reduced oil consumption, faster engine starting (especially in cold weather), and extremely fast lubrication of all moving parts compared to conventional mineral oils. In addition, a special blend of additives protects the engine against harmful deposits and wear.SAE 5w-30 is the preferred viscosity grade of U.S. automobile manufacturers. It exceeds the requirements of API SJ and ILSAC GF-2 and it provides superior performance in extreme cold temperatures. ApplicationsChevron Supreme Synthetic Motor Oils are recommended for all four-stroke gasoline engines in passenger cars, sprot utility vehicles, and light trucks.
Physical Properties Metric English Comments
API Gravity 33.7 °
33.7 °
Viscosity 2400 cP

@Temperature -25.0 °C
2400 cP

@Temperature -13.0 °F
Cold Crank
Viscosity Measurement 161
161
Viscosity Index; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 67.9 cSt
67.9 cSt
ASTM D445
Kinematic Viscosity at 100°C (212°F) 10.4 cSt
10.4 cSt
ASTM D445
Ash 1.12 %
1.12 %
Sulfated Ash wt%
Thermal Properties Metric English Comments
Pour Point <= -52.0 °C
<= -61.6 °F
ASTM D97
Flash Point 240 °C
464 °F
ASTM D92
Component Elements Properties Metric English Comments
Phosphorous, P 0.092 %
0.092 %
Zinc, Zn 0.128 %
0.128 %
Chemical Properties Metric English Comments
Total Base Number 9.0
9.0
ASTM D2896