Material Notes:
Texaco Novatex EP are water resistant, extreme pressure greases. They are manufactured using highly refined, select high viscosity index base oils, a calcium soap, and a specifically selected additive package containing extreme pressure additives as well as corrosion and rust inhibitors.Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.Notes:Minimum operating temperature is the lowest temperature at which a grease, already in place, could be expected to provide lubrication. Most greases cannot be pumped at these minimum temperatures.Maximum operating temperature is the highest temperature at which the grease could be used with frequent (daily) relubrication. Determined on mineral oil extracted by vacuum filtration.CPS Number: 222904; MSDS Number: 9007
Physical Properties Metric English Comments
Viscosity Measurement 62
62
Viscosity Index, See Note 3.
Saybolt Viscosity at 100°F 1104 SUS
1104 SUS
See Note 3.
Saybolt Viscosity at 210°F 80 SUS
80 SUS
See Note 3.
Kinematic Viscosity at 40°C (104°F) 206 cSt
206 cSt
See Note 3.
Kinematic Viscosity at 100°C (212°F) 15 cSt
15 cSt
See Note 3.
Mechanical Properties Metric English Comments
Four Ball Extreme Pressure, Load Wear Index 46
46
Four Ball Extreme Pressure, Weld Load 250 kg
551 lb (mass)
Four Ball Wear 0.400 mm
0.0157 in
Scar Diameter
Penetration P(60), 1/10 mm 325
325
Unknown Amount of Work, 25°C (77°F)
Timken Test 18100 g
40.0 lb
OK Load
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 93.0 °C
199 °F
See Note 2.
Minimum Service Temperature, Air -29.0 °C
-20.2 °F
See Note 1.
Flash Point 162 °C
324 °F
See Note 3.
Dropping Point 260 °C
500 °F
Descriptive Properties Value Comments
Color Brown
Corrosion, Copper Strip 1B
Texture Smooth
Thickener, % 7
Calcium
Water Washout, wt% 2
Loss at 175°F