ChevronTexaco ISO 22 Form Oil

Category Fluid , Lubricant
Manufacturer ChevronTexaco Corp
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ChevronTexaco ISO 22 Form Oil.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
FeaturesChevron Form Oil is a high quality, lightly compounded lubricant which will do an excellent job as a concrete form oil where customers desire a quick clean break from the forms.Chevron Form Oil is a light colored oil manufactured using specially refined base oils. These base oils possess excellent natural low pour points, good "metal wetting" characteristics, and good natural film strength.Chevron Form Oil contains an oiliness additive that improves film strength under boundary lubrication.ApplicationsChevron Form Oil is an excellent concrete form wetting agent. It can be used on any form where a release agent is recommended. Chevron Form Oil is especially recommended for the manufacture of precast concrete structures, concrete pipe, and precast concrete curbs and beams.Chevron Form Oil, with the oiliness additive, does an excellent job in aluminum polishing.Chevron Form Oil is recommended for use by the steel industry as a rust preventive on sheet and plate steel, wire, and cold drawn bar stock in warehouse storage.
Physical Properties Metric English Comments
API Gravity 26.8 °
26.8 °
Viscosity Measurement 56
56
Viscosity Index; ASTM D2270
Saybolt Viscosity at 100°F 121 SUS
121 SUS
Saybolt Viscosity at 210°F 40.1 SUS
40.1 SUS
Kinematic Viscosity at 40°C (104°F) 23.1 cSt
23.1 cSt
ASTM D445
Kinematic Viscosity at 100°C (212°F) 4.1 cSt
4.1 cSt
ASTM D445
Thermal Properties Metric English Comments
Pour Point -40.0 °C
-40.0 °F
ASTM D97
Flash Point 185 °C
365 °F
ASTM D92
Descriptive Properties Value Comments
Wetting Agent, % 4.5