Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ChevronTexaco Hot Punch Compound H

Category Fluid , Lubricant , Calcium Gellant
Manufacturer ChevronTexaco Corp
Trade Name Hot Punch
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ChevronTexaco Hot Punch Compound H.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Texaco Hot Punch Compound H is a dark, semi-fluid calcium soap thickened grease designed for use as a die lubricant. It contains graphite and telc, which enhance its lubricity.Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.Notes:Determined on mineral oil extracted by vacuum filtration.CPS Number: 221979; MSDS Number: 9020
Physical Properties Metric English Comments
Solids Content 43 %
43 %
Saybolt Viscosity at 100°F 3775 SUS
3775 SUS
See Note 1.
Saybolt Viscosity at 210°F 148 SUS
148 SUS
See Note 1.
Kinematic Viscosity at 40°C (104°F) 685 cSt
685 cSt
See Note 1.
Kinematic Viscosity at 100°C (212°F) 30 cSt
30 cSt
See Note 1.
Mechanical Properties Metric English Comments
Penetration P(0), 1/10 mm 415
415
Unworked, 25°C (77°F)
Thermal Properties Metric English Comments
Flash Point 260 °C
500 °F
See Note 1.
Descriptive Properties Value Comments
Color Black
Texture Smooth
Thickener, % 1.5
Calcium
Copyright © lookpolymers.com All Rights Reserved