ChevronTexaco FM Trolley Oil

Category Fluid , Lubricant
Manufacturer ChevronTexaco Corp
Trade Name FM
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ChevronTexaco FM Trolley Oil.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Chevron Trolley Oil FM is a tasteless, odorless, high viscosity index paraffinic lubricating oil combined with additives that provide lubricity and rust protection, antiwear performance, and tackiness to minimize oil drippings.This product provides performance well above that found in typical white mineral oils often used in the food industry.ApplicationsChevron Trolley Oil FM is designed for the lubrication and rust prevention of trolley hooks and bearings in meat processing plants. This lubricant emulsifies readily with caustic solutions to form a detergent that helps to clean animal fat from the trolley hooks. Chevron Trolley Oil FM contains lubricity agents that promote free movement of the trolleys without sticking.
Physical Properties Metric English Comments
API Gravity 32.2 °
32.2 °
Viscosity Measurement 120
120
ASTM D2270
Saybolt Viscosity at 100°F 226 SUS
226 SUS
Saybolt Viscosity at 210°F 49.9 SUS
49.9 SUS
Kinematic Viscosity at 40°C (104°F) 44 cSt
44 cSt
ASTM D445
Kinematic Viscosity at 100°C (212°F) 7.1 cSt
7.1 cSt
ASTM D445
Thermal Properties Metric English Comments
Pour Point -14.0 °C
6.80 °F
ASTM D97
Flash Point 226 °C
439 °F
ASTM D92