ChevronTexaco Aero SAE 60/Grade 120 Engine Oil Uncompounded

Category Fluid , Lubricant
Manufacturer ChevronTexaco Corp
Trade Name Aero
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ChevronTexaco Aero SAE 60/Grade 120 Engine Oil Uncompounded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
FeaturesChevron Aero Engine Oils Uncompounded are a blend of high quality base oil, with small amounts of viscosity modifier for improved fluidity at cold temperatures, antioxidant, and antifoam agent.Chevron Aero Engine Oils Uncompounded do not contain ashless dispersant additives that retard the formation of sludge.Chevron Aero Engine Oils Uncompounded are designed for the lubrication of aircraft piston engines where a straight mineral oil is recommended.ApplicationsChevron Aero Engine Oils Uncompounded are the type of oil recommended by most engine manufacturers and engine rebuilders for use as a break-in oil for new,rebuilt or overhauled four-stroke cycle aircraft piston engines. Check with the engine manufacturer or overhaul facility for their specific recommendation. They fully meet the requirements of SAE J1966, which has replaced MIL-L-6082E as the standard for nondispersant oils.
Physical Properties Metric English Comments
API Gravity 27.5 °
27.5 °
Viscosity Measurement 93
93
Viscosity Index; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 333 cSt
333 cSt
ASTM D445
Kinematic Viscosity at 100°C (212°F) 24.2 cSt
24.2 cSt
ASTM D445
Ash 0.00 %
0.00 %
Sulfated Ash wt%
Thermal Properties Metric English Comments
Pour Point -12.0 °C
10.4 °F
ASTM D97
Flash Point 296 °C
565 °F
ASTM D92