Material Notes:
Texaco Gas Turbine oils deliver value through:Superior oxidation stability for long service life at elevated temperatures.Rust and corrosion protectionHigh viscosity index for minimum viscosity change when variations in temperature occur.Minimum foam prevents sump overflow or erratic governor operation.Fast air release minimizes possibility of pump cavitation in systems with high circulation rates and small reservoirs.Superior thermal stability minimizes deposit formation.Rapid water separation keeps water in oil to a minimum.Hydraulic fluid service — Texaco Gas Turbine 32 and 46 are excellent hydraulic fluids in low pressure systems up to 1000 psi.Environmental benefits — These oils are ashless. This facilitates reclaiming and recycling of the used oils. They are not expected to be harmful to aquatic organisms.Texaco Gas Turbine oils are designed to meet the critical demands of stationary gas turbines and high temperature, high pressure steam turbines. They are an excellent recommendation for equipment used in combined cycle plants. They are ideal for many other industrial applications including air compression.Higher temperatures in the advanced gas and steam turbines require a circulating system oil with exceptional high temperature stability. Texaco Gas Turbine oils provide outstanding oxidation and corrosion inhibition and excellent air release and foam suppression. Texaco Gas Turbine oils provide long lubricant life and reduced equipment wear.Texaco Gas Turbine oils are recommended for use in gas and steam turbines. The following viscosity grades are formulated to meet the specified OEM requirements: Texaco Gas Turbine 32 meets:General Electric GEK-32568f, GEK 28143ASolar ES 9 224 requirements for gas turbine oilsCincinnati Machine P 38Alstom Power HTGD 90117Siemens TLV 9013Texaco Gas Turbine 46 meetsSolar ES 9 224 requirements for gas turbine oilsCincinnati Machine P 55Alstom Power HTGD 90117Siemens TLV 9013Do not use in high pressure systems in the vicinity of flames, sparks and hot surfaces. Use only in well ventilated areas. Keep container closed. Do not use in breathing air apparatus or medical equipment.Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing. CPS Number: 223388; MSDS Number: 8613
Physical Properties Metric English Comments
API Gravity 32.7 °
32.7 °
Viscosity Measurement 102
102
Viscosity Index
Saybolt Viscosity at 100°F 157 SUS
157 SUS
Saybolt Viscosity at 210°F 43.8 SUS
43.8 SUS
Kinematic Viscosity at 40°C (104°F) 30.4 cSt
30.4 cSt
Kinematic Viscosity at 100°C (212°F) 5.2 cSt
5.2 cSt
Oxidative Stability 36 hour
36 hour
to 25 psi drop; ASTM D2272
10000 hour
10000 hour
Hours to 2 mg KOH/g acid number; ASTM D943
Thermal Properties Metric English Comments
Pour Point -36.0 °C
-32.8 °F
Flash Point 222 °C
432 °F
Users viewing this material also viewed the following: