Material Notes:
Texaco Military Symbol Oil 2190 T-EP delivers value through:Long lubricant life because of selected base stocks and additives.Extreme pressure characteristics that provide high film strength to protect gears and bearings engaged in severe, heavy-duty service.MIL-L-17331H(SH) qualified — Meets stringent military specifications.High viscosity index — Minimal viscosity change in broad operating temperature range enhances lubricant film strength.Texaco Military Symbol Oil 2190 T-EP was developed primarily as a circulating system oil for marine gear turbine sets.Texaco Military Symbol Oil 2190 T-EP provides mild extreme pressure protection as well as resistance to rust, oxidation, corrosion, and foaming.Texaco Military Symbol Oil 2190 T-EP has outstanding thermal and oxidation stability that allows it to withstand the high temperatures found in turbine bearing and gear lubrication.The foam inhibition prevents the buildup of foam in the sump tank with possible vent pipe overflow.Its excellent stability, high viscosity index, and rust and corrosion inhibition assures high film strength lubrication for gears and bearings, as well as rust and corrosion protection. Together, these qualities mean both long lubricant and equipment life.Texaco Military Symbol Oil 2190 T-EP is recommended for use in marine turbine reduction gears, where heavy tooth loading and shock loads are encountered.The extreme pressure properties enable Texaco Military Symbol Oil 2190 T-EP to meet the requirements of MIL-L-17331H(SH) Amendment 3, Symbol 2190 TEP.Do not filter through Fullers Earth-type filtration systems since this would deplete the additive package.Do not use in high pressure systems in the vicinity of flames, sparks and hot surfaces. Use only in well ventilated areas. Keep container closed.Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing. CPS Number: 221546; MSDS Number: 8695
Physical Properties Metric English Comments
API Gravity 31.9 °
31.9 °
Viscosity Measurement 99
99
Viscosity Index
Saybolt Viscosity at 100°F 415 SUS
415 SUS
Saybolt Viscosity at 210°F 59.1 SUS
59.1 SUS
Kinematic Viscosity at 40°C (104°F) 79.8 cSt
79.8 cSt
Kinematic Viscosity at 100°C (212°F) 9.7 cSt
9.7 cSt
Ash <= 0.0010 %
<= 0.0010 %
Sulfated Ash
ASTM Color 0.50
0.50
ASTM D1500
Thermal Properties Metric English Comments
Pour Point -12.0 °C
10.4 °F
Flash Point 246 °C
475 °F
Chemical Properties Metric English Comments
Acid Value 0.16
0.16
mg KOH/g; ASTM D974
Descriptive Properties Value Comments
Conradson Carbon Residue, mass% 0.1
Corrosion, Copper Strip 1
3 h at 100°C
Rust Prevention Pass
48 h, Oil water washed