Chevron Phillips Xtel® XK2340 Polyphenylene Sulfide Alloy

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS) , Polyphenylene Sulfide (PPS) Alloy, Glass Reinforced, Flow Enhanced
Manufacturer Chevron Phillips Chemical Company LP
Trade Name Xtel®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chevron Phillips Xtel® XK2340 Polyphenylene Sulfide Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Black Polyphenylene Sulfide AlloyXtel™ XK2340 is a high performance, glass fiber reinforced, PPS-based alloy developed to provide excellent mechanical strength with an unique blend of toughness and rigidity along with excellent flow in thin-walled parts, low flash characteristics, and fast cycle times. Xtel™ XK2340 can be easily molded in conventional injection molding equipment utilizing water heated molds.Comments: Test specimen molding conditions: Stock Temperature, 280-305°C; Mold Temperature, 80°C; ASTM Values Converted to SI UnitsData provided by Chevron Phillips Chemical Company LP.
Physical Properties Metric English Comments
Density 1.55 g/cc
0.0560 lb/in³
ASTM D792
Water Absorption 0.030 %
0.030 %
ASTM D570
Linear Mold Shrinkage 0.0030 cm/cm
0.0030 in/in
102 mm X 102 mm X 3.2 mm Plaques, Edge Gated
Linear Mold Shrinkage, Transverse 0.0060 cm/cm
0.0060 in/in
Measured on 102 mm X 102 mm X 3.2 mm Plaques, Edge Gated
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 180 MPa
26100 psi
ASTM D638
Elongation at Break 1.9 %
1.9 %
ASTM D638
Flexural Yield Strength 250 MPa
36300 psi
ASTM D790
Flexural Modulus 13.0 GPa
1890 ksi
ASTM D790
Compressive Yield Strength 220 MPa
31900 psi
ASTM D695
Izod Impact, Notched 0.900 J/cm
1.69 ft-lb/in
ASTM D256
Izod Impact, Unnotched 6.90 J/cm
12.9 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 22.0 µm/m-°C

@Temperature -50.0 - 50.0 °C
12.2 µin/in-°F

@Temperature -58.0 - 122 °F
Axial; ASTM E831
39.0 µm/m-°C

@Temperature 100 - 200 °C
21.7 µin/in-°F

@Temperature 212 - 392 °F
Axial; ASTM E831
CTE, linear, Transverse to Flow 63.0 µm/m-°C

@Temperature 20.0 °C
35.0 µin/in-°F

@Temperature 68.0 °F
ASTM E831
110 µm/m-°C

@Temperature 100 - 200 °C
61.1 µin/in-°F

@Temperature 212 - 392 °F
ASTM E831
Deflection Temperature at 1.8 MPa (264 psi) 245 °C
473 °F
ASTM D648
Electrical Properties Metric English Comments
Dielectric Constant 4.0

@Frequency 1e+6 Hz
4.0

@Frequency 1e+6 Hz
ASTM D150
4.5

@Frequency 1000 Hz
4.5

@Frequency 1000 Hz
ASTM D150
Dielectric Strength 27.0 kV/mm
686 kV/in
ASTM D149
Dissipation Factor 0.018

@Frequency 1e+6 Hz
0.018

@Frequency 1e+6 Hz
ASTM D150
0.030

@Frequency 1000 Hz
0.030

@Frequency 1000 Hz
ASTM D150
Arc Resistance 116 sec
116 sec
ASTM D495
Comparative Tracking Index 275 V
275 V
UL 746A