Material Notes:
Xtel® XE5030BL is a high performance, glass fiber reinforced, PPS based alloy developed to provide high ductility and impact strength along with good thermal stability.Information provided by Chevron PhillipsMeasured on 102mm x 102mm x 3.2 mm plaques, edge gated.
Physical Properties Metric English Comments
Density 1.50 g/cc
0.0542 lb/in³
ISO 1183A
Water Absorption 0.050 %
0.050 %
ASTM D-570
Linear Mold Shrinkage, Flow 0.0020 cm/cm
0.0020 in/in
Linear Mold Shrinkage, Transverse 0.0060 cm/cm
0.0060 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Yield 140 MPa
20300 psi
ISO 527
Elongation at Yield 2.1 %
2.1 %
ISO 527
Flexural Strength 200 MPa
29000 psi
ISO 178
Flexural Modulus 8.50 GPa
1230 ksi
ISO 178
Compressive Strength 210 MPa
30500 psi
ISO 604
Izod Impact, Notched (ISO) 9.00 kJ/m²
4.28 ft-lb/in²
ISO 180A
Izod Impact, Unnotched (ISO) 45.0 kJ/m²
21.4 ft-lb/in²
ISO 180A
Thermal Properties Metric English Comments
CTE, linear 15.0 µm/m-°C

@Temperature 100 - 200 °C
8.33 µin/in-°F

@Temperature 212 - 392 °F
Axial; ISO 11359-2
20.0 µm/m-°C

@Temperature -50.0 - 50.0 °C
11.1 µin/in-°F

@Temperature -58.0 - 122 °F
Axial; ISO 11359-2
CTE, linear, Transverse to Flow 65.0 µm/m-°C

@Temperature -50.0 - 50.0 °C
36.1 µin/in-°F

@Temperature -58.0 - 122 °F
ISO 11359-2
130 µm/m-°C

@Temperature 100 - 200 °C
72.2 µin/in-°F

@Temperature 212 - 392 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 250 °C
482 °F
ISO 75
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
ASTM D-257
Dielectric Constant 3.5

@Frequency 1e+6 Hz
3.5

@Frequency 1e+6 Hz
ASTM D-150
3.6

@Frequency 1000 Hz
3.6

@Frequency 1000 Hz
ASTM D-150
Dielectric Strength 20.0 kV/mm
508 kV/in
ASTM D-149
Dissipation Factor 0.0040

@Frequency 1000 Hz
0.0040

@Frequency 1000 Hz
ASTM D-150
0.0090

@Frequency 1e+6 Hz
0.0090

@Frequency 1e+6 Hz
ASTM D-150
Arc Resistance 120 sec
120 sec
ASTM D-495
Comparative Tracking Index 150 V
150 V
UL 746A
Processing Properties Metric English Comments
Melt Temperature 315 - 345 °C
599 - 653 °F
Mold Temperature 135 °C
275 °F
Users viewing this material also viewed the following: