Chevron Phillips Marlex® M362 LLDPE Pipe and Corrugated Extrusion Resin  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Extrusion Grade
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chevron Phillips Marlex® M362 LLDPE Pipe and Corrugated Extrusion Resin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Characteristics: Good long-term hoop strengthExtended outdoor lifeClean N550 carbon blackApplications: PipesNot recommended for contact with food productsInformation provided by Chevron Phillips.
Physical Properties Metric English Comments
Density 0.944 g/cc
0.0341 lb/in³
Base Density; ASTM D1505
Carbon Black Loading 31 %
31 %
ASTM D1603
Melt Flow 3.0 g/10 min
3.0 g/10 min
Condition 190/2.16; ASTM D1238
Melt Index of Compound 0.11 g/10 min
0.11 g/10 min
Condition 190/21.6, HLMI; ASTM D1238