Chevron Phillips Marlex® M248 LLDPE Carbon Black Concentrate

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Compounding Resin
Manufacturer Chevron Phillips Chemical Company LP
Trade Name Marlex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chevron Phillips Marlex® M248 LLDPE Carbon Black Concentrate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Characteristics: excellent thermal stability, a long useful outdoor life, good processabilityApplications: geomembranes, sheets and thermoforming, blow moldingProcessing: 192-232°C stock temperature depending on base resin used. The actual temperature profile will depend on the extrusion conditions. To achieve 2.5% carbon black level, the correct let down ratio is 9:1Information provided by Chevron Phillips Chemical Company.
Processing Properties Metric English Comments
Processing Temperature 192 - 232 °C
378 - 450 °F
Stock temperature depending on base resin used