Chevron Phillips Marlex® HHM 5502 BZ High Density Ethylene Hexene Copolymer

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Injection Molded
Manufacturer Chevron Phillips Chemical Company LP
Trade Name Marlex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chevron Phillips Marlex® HHM 5502 BZ High Density Ethylene Hexene Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High Density Ethylene Hexene CopolymerCustomer Benefits: This resin eliminates the need for a mold release agent at machine side. Incorporation of zinc stearate at resin extrusion assures uniform, consistent release properties.Applications: Injection blow moldingProcessing Recommendations:Melting Temperature: Upper Limit: 260°C, Lower Limit: 232°CSpecification Data: ASTM D4976 - PE 235. ASTM D1248 - Type III, Class A, Category 5. FDA Regulation 177.1520(c)3.2. Suitable for food packaging. Limited to application temperatures of 100°C and below (Condition B-H, Table 2,21 CFR 176.170). Listed in Drug Master FileData provided by Chevron Phillips Chemical Company, LP.
Physical Properties Metric English Comments
Density 0.955 g/cc
0.0345 lb/in³
ASTM D1505
Environmental Stress Crack Resistance 45 hour
45 hour
Condition A, F<sub>50</sub>, 100% Igepal CO-630, ASTM D1693; Condition B, F<sub>50</sub>: 35
Melt Flow 0.35 g/10 min
0.35 g/10 min
Condition 190/2.16; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 28.0 MPa
4060 psi
2 in per min; ASTM D638 Type IV
Elongation at Break >= 600 %
>= 600 %
2 in per min; ASTM D638 Type IV
Processing Properties Metric English Comments
Processing Temperature 232 - 260 °C
450 - 500 °F
Copyright © lookpolymers.com All Rights Reserved