Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chevron Phillips Marlex® HHM 5202LD HDPE Blow Molding Resin  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Blow Molding Grade
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chevron Phillips Marlex® HHM 5202LD HDPE Blow Molding Resin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Resin Type: Hexene CopolymerCharacteristics: Good stiffnessExceptional processabilityGood ESCRApplications: Household & industrial chemical containersInformation provided by Chevron Phillips.
Physical Properties Metric English Comments
Density 0.951 g/cc
0.0344 lb/in³
ASTM D1505
ESCR 100% Igepal® 50 hour
50 hour
Conditions A and B; ASTM D1693
Melt Index of Compound 0.35 g/10 min
0.35 g/10 min
Condition 190/2.16; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 26.0 MPa
3770 psi
2 in/min, Type IV bar; ASTM D638
Elongation at Break 600 %
600 %
2 in/min, Type IV bar; ASTM D638
Flexural Modulus 1.31 GPa
190 ksi
Tangent, 16:1 span:depth,0.5in/min; ASTM D790
Thermal Properties Metric English Comments
Brittleness Temperature <= -75.0 °C
<= -103 °F
Type A clamp, type 1 specimen; ASTM D746