Chevron Phillips Marlex® EHM 6007 High Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Blow Molding Grade
Manufacturer Chevron Phillips Chemical Company LP
Trade Name Marlex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chevron Phillips Marlex® EHM 6007 High Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High Density PolyethyleneCustomer Benefits: A blow molding grade rein that offers a high quality product for those critical food packaging jobs and good impact strength and stiffness.Applications: Lightweight containers for bottling products such as milk, distilled water, soft drink concentrate, and fruit juice.Processing Recommendations:Melting Temperature: Upper Limit: 226°C, Lower Limit: 171°CSpecification Data: ASTM D4976 - PE 235. ASTM D1248 - Type IV, Class A, Category 4. Meets FDA regulation 177.1520. Suitable for food packaging applications.Data provided by Chevron Phillips Chemical Company, LP.
Physical Properties Metric English Comments
Density 0.964 g/cc
0.0348 lb/in³
ASTM D1505
Environmental Stress Crack Resistance 15 hour
15 hour
Condition A, F<sub>50</sub> 100% Igepal CO-630, ASTM D1693; Condition B, F<sub>50</sub>: 10, ASTM D1693
Melt Flow 0.65 g/10 min
0.65 g/10 min
Condition 190/2.16; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 30.0 MPa
4350 psi
2 in per min; ASTM D638 Type IV
Elongation at Break >= 300 %
>= 300 %
2 in per min; ASTM D638 Type IV
Flexural Modulus 1.654 GPa
239.9 ksi
ASTM D790
Thermal Properties Metric English Comments
Brittleness Temperature <= -118 °C
<= -180 °F
ASTM D746
Processing Properties Metric English Comments
Processing Temperature 171 - 226 °C
340 - 439 °F