Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Blow Molding Grade
Manufacturer Chevron Phillips Chemical Company LP
Trade Name Marlex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chevron Phillips Marlex® EHM 6004 High Density Polyethylene, Blow Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This high molecular weight, ethylene homopolymer is tailored for lightweight blow molded containers that:Require excellent stiffnessRequire exceptional processabilityAre durable and recyclable for sustainabilityTypical blow molded applications for EHM 6004 include:Dairy bottlesLiquid food packagingCaulking tubesThis resin meets these specifications:ASTM D4976 - PE 245FDA 21 CFR 177.1520(c) 2.2, use conditions B through H per 21 CFR 176.170(c)Information provided by Chevron Phillips Chemical Company LP.
Physical Properties Metric English Comments
Specific Gravity 0.963 g/cc
0.963 g/cc
ASTM D1505
ESCR 100% Igepal® 15 hour
15 hour
Condition B, F50; ASTM D1693
Melt Flow 0.37 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.37 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 31.0 MPa
4500 psi
2 in/min, Type IV bar; ASTM D638
Elongation at Break 500 %
500 %
2 in/min, Type IV bar; ASTM D638
Flexural Modulus 1.65 GPa
239 ksi
Tangent; ASTM D790
Thermal Properties Metric English Comments
Brittleness Temperature <= -75.0 °C
<= -103 °F
Type A clamp, Type I Specimen; ASTM D746