Material Notes:
High density polyethylene. This gas phase, high molecular weight hexene copolymer is tailored for lightweight blow molded applications that: Require excellent stiffness to ESCR ratioRequire good melt strengthAre durable and recyclable for sustainability Applications: Typical blow molded applications for 9514H include: Household and industrial chemical containersLarge partsInformation provided by PhillipsThis resin meets these specifications: ASTM D4976 - PE 235FDA 21 CFR 177.1520(c) 3.2a, use conditions B through H per 21 CFR 176.170(c)
Physical Properties Metric English Comments
Density 0.957 g/cc
0.0346 lb/in³
ASTM D-1505
ESCR 100% Igepal® 50 hour
50 hour
Condition B, F50; ASTM D-1693
Melt Index of Compound 0.30 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.30 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D-1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 30.0 MPa
4350 psi
2 in/min, Type IV bar; ASTM D-638
Elongation at Break 800 %
800 %
2 in/min, Type IV bar; ASTM D-638
Flexural Modulus 1.41 GPa
205 ksi
Tangent - 16:1 span:depth, 0.5 in/min; ASTM D-790
Thermal Properties Metric English Comments
Brittleness Temperature <= -75.0 °C
<= -103 °F
Type A, Type I specimen; ASTM D-746