Chevron Phillips Marlex® 9509HF High Density Polyethylene, Blow Molding

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Blow Molding Grade
Manufacturer Chevron Phillips Chemical Company LP
Trade Name Marlex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chevron Phillips Marlex® 9509HF High Density Polyethylene, Blow Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This gas phase, high molecular weight, hexane copolymer with synthetic antistatic agent is tailored for lightweight blow molded applications that:Require outstanding ESCRRequire excellent impact resistanceAre durable and recyclable for sustainabilityTypical blow molded applications for 9505HF include:Detergent bottlesHousehold and industrial chemical containersIndustrial containers / Large partsThis resin meets these specifications:ASTM D4976 - PE 235FDA 21 CFR 177.1520(c) 3.2a, use conditions B through H per 21 CFR 176.170(c)Information provided by Chevron Phillips Chemical Company LP.
Physical Properties Metric English Comments
Specific Gravity 0.949 g/cc
0.949 g/cc
ASTM D1505
ESCR 100% Igepal® 250 hour
250 hour
Condition B, F50; ASTM D1693
Melt Flow 0.34 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.34 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 26.0 MPa
3770 psi
2 in/min, Type IV bar; ASTM D638
Elongation at Break 500 %
500 %
2 in/min, Type IV bar; ASTM D638
Flexural Modulus 1.07 GPa
155 ksi
Tangent; ASTM D790
Thermal Properties Metric English Comments
Brittleness Temperature <= -75.0 °C
<= -103 °F
Type A clamp, Type I Specimen; ASTM D746