Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chevron Phillips Marlex® 9503HF High Performance Series HDPE Blow Molding Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Blow Molding Grade
Manufacturer Chevron Phillips Chemical Company LP
Trade Name Marlex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chevron Phillips Marlex® 9503HF High Performance Series HDPE Blow Molding Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Resin Type: linear copolymerCharacteristics: outstanding ESCR, excellent impact resistance, medium molecular weight distribution, wide range of processing conditions, high melt strength, good parison uniformity, good trimming characteristics. Federal specification LP390C Classification Type I, Class H, Grades (1-5), Category 5. Meets FDA Regulation 21CFR 177.1520. Some restrictions apply when containing an antistatic additive.Applications: hard to hold chemicals, household-industrial chemical containers, detergentsBurn rate < 5 cm/min.Information provided by Chevron Phillips Chemical Company.
Physical Properties Metric English Comments
Density 0.946 g/cc
0.0342 lb/in³
ASTM D1505
Apparent Bulk Density 0.590 g/cc
0.0213 lb/in³
ASTM D1895
Melt Flow 0.27 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.27 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
ASTM D2240
Tensile Strength, Yield 24.8 MPa
3600 psi
ASTM D638
Elongation at Break >= 500 %
>= 500 %
ASTM D638
Flexural Modulus 0.900 GPa
131 ksi
1% Secant; ASTM D 790
Tensile Impact Strength 135 kJ/m²
64.2 ft-lb/in²
S bar; ASTM D 1822
Thermal Properties Metric English Comments
Vicat Softening Point 123 °C
253 °F
ASTM D1525
Brittleness Temperature <= -75.0 °C
<= -103 °F
ASTM D746