Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chevron Phillips Marlex® 9398 HDPE Pipe and Corrugated Extrusion Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Extruded
Manufacturer Chevron Phillips Chemical Company LP
Trade Name Marlex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chevron Phillips Marlex® 9398 HDPE Pipe and Corrugated Extrusion Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Resin Type: Hexene CopolymerCharacteristics: Good melt strengthExcellent ESCRApplications: ConduitDuctInformation provided by Chevron Phillips.
Physical Properties Metric English Comments
Density 0.945 g/cc
0.0341 lb/in³
ASTM D1505
ESCR 100% Igepal® >= 2000 hour
>= 2000 hour
Condition C; ASTM D1693
ESCR 10% Igepal® >= 2000 hour
>= 2000 hour
Condition B; ASTM D1693
Melt Flow 11 g/10 min
11 g/10 min
Condition 190/21.6, HLMI; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 22.0 MPa
3190 psi
2 in/min, Type IV bar; ASTM D638
Elongation at Break 800 %
800 %
2 in/min, Type IV bar; ASTM D638
Flexural Modulus 0.900 GPa
131 ksi
2% Secant; ASTM D790
Thermal Properties Metric English Comments
Brittleness Temperature <= -75.0 °C
<= -103 °F
Type A clamp, type 1 specimen; ASTM D746
Copyright © lookpolymers.com All Rights Reserved