Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chevron Phillips Marlex® 9346 HDPE Natural Pipe Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Pipe Grade
Manufacturer Chevron Phillips Chemical Company LP
Trade Name Marlex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chevron Phillips Marlex® 9346 HDPE Natural Pipe Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Resin Type: Linear Copolymer; PE3408 Pipe Resin; ASTM D 3350 Classification:345464C when used with an approved color concentrate; ASTM D 4976 Classification: PE 235, A 56607Applications:Pressure Piping ApplicationsData provided by Chevron Chemical.
Physical Properties Metric English Comments
Density 0.946 g/cc
0.0342 lb/in³
ASTM D1505
Environmental Stress Crack Resistance >= 1500 hour

@Temperature 50.0 °C
>= 1500 hour

@Temperature 122 °F
F<sub>50</sub>, Cond. B.; ASTM D1693
>= 1500 hour

@Temperature 100 °C
>= 1500 hour

@Temperature 212 °F
F<sub>50</sub> Cond. C; ASTM D 1693
High Load Melt Index 9.0 g/10 min

@Load 21.6 kg,
Temperature 190 °C
9.0 g/10 min

@Load 47.6 lb,
Temperature 374 °F
High Load; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 66
66
ASTM D2240
Tensile Strength, Ultimate 34.0 MPa
4930 psi
ASTM D638
Tensile Strength, Yield 22.0 MPa
3190 psi
ASTM D638
Elongation at Break >= 800 %
>= 800 %
ASTM D638
Flexural Modulus 0.900 GPa
131 ksi
3 pt. secant. ASTM D790
Thermal Properties Metric English Comments
Vicat Softening Point 126 °C
259 °F
ASTM D1525
Brittleness Temperature <= -59.0 °C
<= -74.2 °F
ASTM D746