Chevron Phillips MarFlex® 5628 LDPE Blown Film Resin

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Film Grade
Manufacturer Chevron Phillips Chemical Company LP
Trade Name MarFlex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chevron Phillips MarFlex® 5628 LDPE Blown Film Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Resin Type: HomopolymerCharacteristics: Superior tensile and impact strengthGood abrasion and tear resistanceExcellent retention of properties after agingApplications: LaminationsPallet shrinkcase shrink wrapHeavy duty packagingC&A film and container linersInformation provided by Chevron Phillips.
Physical Properties Metric English Comments
Density 0.922 g/cc
0.0333 lb/in³
ASTM D1505
Thickness 76.2 microns
3.00 mil
Melt Index of Compound 0.40 g/10 min
0.40 g/10 min
ASTM D1238E
Mechanical Properties Metric English Comments
Secant Modulus, MD 0.165 GPa
23.9 ksi
ASTM D882
Secant Modulus, TD 0.179 GPa
26.0 ksi
ASTM D882
Coefficient of Friction 0.50
0.50
ASTM D1894
Dart Drop 3.94 g/micron
100 g/mil
2" Dart, 60" Drop Height; ASTM D1709
Optical Properties Metric English Comments
Haze 7.0 %
7.0 %
ASTM D1003
Gloss 57 %
57 %
45°; ASTM D2457
90 %
90 %
60°; ASTM D2457
Processing Properties Metric English Comments
Melt Temperature 210 °C
410 °F
Die Opening 0.0762 cm
0.0300 in
Extruder Size 6.35 cm
2.50 in
Blow-up Ratio (BUR) 3.0
3.0
Descriptive Properties Value Comments
Antiblock Low
Users viewing this material also viewed the following: