Material Notes:
K-Resin® Styrene-Butadiene Copolymer (SBC)Applications:Thermoformed clam shell packagingThermoformed blister packsThermoformed medical traysBlow molded productsFeatures:Good clarityGood stiffnessGood formabilityGood toughnessHigh surface glossInformation provided by Chevron Phillips
Physical Properties Metric English Comments
Specific Gravity 1.01 g/cc
1.01 g/cc
ASTM D-792
Melt Flow 6.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
6.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D-1238
Mechanical Properties Metric English Comments
Hardness, Shore D 57
57
ASTM D-2240
Tensile Strength, Yield 21.0 MPa
3050 psi
Type 1 @ 2.0 in/min; ASTM D-638
Elongation at Break 350 %
350 %
ASTM D-638
Flexural Strength 34.0 MPa
4930 psi
1.0 in/min; 0.125" thickness; ASTM D-790
Flexural Modulus 1.05 GPa
152 ksi
1.0 in/min; 0.125" thickness; ASTM D-790
Izod Impact, Notched 0.283 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
0.530 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D-256
Impact Test 44.0 J

@Thickness 3.17 mm,
Temperature 22.8 °C
32.5 ft-lb

@Thickness 0.125 in,
Temperature 73.0 °F
150 in/sec; ASTM D-3763
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 51.0 °C
124 °F
ASTM D-648
Vicat Softening Point 76.0 °C
169 °F
ASTM D-1525
Optical Properties Metric English Comments
Transmission, Visible 92 %
92 %
ASTM D-1003