Chevron Phillips K-Resin® KR01BR SBC  (discontinued **)

Category Polymer , Thermoplastic , Styrene-Butadiene
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chevron Phillips K-Resin® KR01BR SBC  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
K-Resin® Styrene-Butadiene Copolymer (SBC)Applications:Molded boxes with integral hingesMedical devicesDisplaysToysMedia packagingFeatures:Good stiffnessGood toughnessGood warpage resistanceExcellent clarity with a slight blue tintEnhanced mold release characteristicsInformation provided by Chevron Phillips
Physical Properties Metric English Comments
Specific Gravity 1.01 g/cc
1.01 g/cc
ASTM D-792
Melt Flow 8.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
8.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D-1238
Mechanical Properties Metric English Comments
Hardness, Shore D 64
64
ASTM D-2240
Tensile Strength, Yield 34.0 MPa
4930 psi
2.0 in/min; ASTM D-638
Elongation at Yield 25 %
25 %
2.0 in/min; ASTM D-638
Flexural Strength 55.0 MPa
7980 psi
1.0 in/min; 0.125" thickness; ASTM D-790
Flexural Modulus 1.70 GPa
247 ksi
1.0 in/min; 0.125" thickness; ASTM D-790
Impact Test 0.400 J

@Thickness 3.17 mm,
Temperature 22.8 °C
0.295 ft-lb

@Thickness 0.125 in,
Temperature 73.0 °F
150 in/sec; ASTM D-3763
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 64.0 °C
147 °F
ASTM D-648
Vicat Softening Point 90.0 °C
194 °F
ASTM D-1525
Optical Properties Metric English Comments
Gloss 148 %
148 %
60°, mold temp 100°F; ASTM D-2457
Transmission, Visible 93 %
93 %
ASTM D-1003
Processing Properties Metric English Comments
Mold Temperature 37.8 °C
100 °F