Chevron Phillips 5102 LDPE Injection Blow Molding Resin  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Blow Molding Grade
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chevron Phillips 5102 LDPE Injection Blow Molding Resin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Resin Type: HomopolymerCharacteristics: Good Core Pin Release, Good Stability, Low Taste and Odor Characteristics, Good Impact and Toughness, Good Clarity on GlossApplications:Squeeze Bottles, Personal Care, Flexible Toys, Adhesives, Toiletries, Food and Drink Bottles, Pharmaceuticals. Burn Rate
Physical Properties Metric English Comments
Density 0.923 g/cc
0.0333 lb/in³
ASTM D1505
Apparent Bulk Density 0.526 g/cc
0.0190 lb/in³
ASTM D1895
Melt Flow 2.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D 1238
Mechanical Properties Metric English Comments
Hardness, Shore D 56
56
ASTM D2240
Tensile Strength, Yield 17.2 MPa
2490 psi
ASTM D638
Elongation at Break >= 600 %
>= 600 %
ASTM D638
Flexural Modulus 0.185 GPa
26.8 ksi
3 pt. secant. ASTM D790
Thermal Properties Metric English Comments
Vicat Softening Point 102 °C
216 °F
ASTM D1525
Brittleness Temperature <= -70.0 °C
<= -94.0 °F
ASTM D746