Material Notes:
Chesterton® KPC 820 is the premium product of choice when searching for an environmentally compliant solution to the plant’s degreasing needs. It is an oil and grease cutting liquid, completely miscible in water. Containing no chlorinated solvents, caustic, buytl compounds, phosphate or petroleum distillates, Chesterton KPC 820 is the safe alternative for all degreasing applications. Chesterton KPC 820 will provide efficiency not usually seen in other “safe” cleaners. It quickly removes metal working fluids of all kinds, grease, grime and other soils common to industrial production areas. When used at elevated temperatures, the cleaning action is accelerated. The heaviest grime can be removed easily at temperatures of 60°C to 82°C. Chesterton KPC 820 is cost efficient. To meet individual cleaning requirements and determine needed solution strengths, field evaluation is necessary. The heaviest industrial grime may require a more concentrated solution, while light soils can be removed with as little as 1-2% concentration.Features:NonflammableNontoxicBiodegradablePhosphate freeHighly dilutableSafe on most metalsNSF A1 – Registration number 133963No offensive odorModerate pHInformation provided by Chesterton
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc
1.04 g/cc
pH 9.9
9.9
Concentrate
Thermal Properties Metric English Comments
Melting Point 0.000 °C
32.0 °F
Freezing Point
Boiling Point 100 °C
212 °F
Descriptive Properties Value Comments
Appearance Clear, transparent liquid
Base Green